Por favor, use este identificador para citar o enlazar este ítem: http://hdl.handle.net/20.500.14076/13810
Registro completo de metadatos
Campo DC Valor Lengua/Idioma
dc.contributor.authorPaucar Cuba, Karín-
dc.contributor.authorRojas Flores, Hugo-
dc.contributor.authorVergara Sotomayor, Abel Fernando-
dc.creatorVergara Sotomayor, Abel Fernando-
dc.creatorVergara Sotomayor, Abel Fernando-
dc.date.accessioned2018-09-18T18:17:13Z-
dc.date.available2018-09-18T18:17:13Z-
dc.date.issued2012-12-01-
dc.identifier.citationPaucar Cuba, K., Rojas Flores, H., & Vergara Sotomayor, A. (2012). Estudio de la resistencia a la corrosión del Aluminio 6063 anodizado. TECNIA, 22(2). https://doi.org/10.21754/tecnia.v22i2.77es
dc.identifier.issn2309-0413-
dc.identifier.urihttp://hdl.handle.net/20.500.14076/13810-
dc.description.abstractEl estudio de la resistencia a la corrosión del anodizado de una aleación de aluminio (AA6063) en ácido sulfúrico a diferentes tiempos de anodizado: 30, 45 y 60 min. se realizó usando la espectroscopia de impedancia electroquímica (EIE) y el ensayo de niebla salina ácida. (ASTM B287). Los datos obtenidos por EIE y su correlación con los circuitos equivalentes más apropiados permitieron determinar los parámetros asociados a la capa porosa y a la capa barrera del óxido protector formado sobre la superficie del aluminio en estudio. La exposición de las muestras anodizadas durante 250h a una niebla salina ácida permitió observar variaciones en su masa. De los resultados obtenidos por EIE y las pérdidas de masa de las muestras anodizadas se estableció que la película de anodizado de 45 minutos mostró una mayor resistencia a la corrosión en comparación con la obtenida a 60 y 30 min., respectivamente.es
dc.description.abstractThe study of the corrosion resistance of anodized on aluminum alloy (AA6063) in sulfuric acid to different times: 30, 45 and 60 min. was performed using electrochemical impedance spectroscopy (EIS) and the acid salt spray test (ASTM B287). The EIS’data and its correlation with the most appropriate equivalent circuits allowed to determine the parameters associated with the porous layer and the oxide layer protective barrier formed on the aluminum surface under study. Exposure of the samples anodized for a 250h salt spray acid allowed to observe changes in their mass. From the results obtained by EIS and the mass losses of the anodized samples was established that the anodized film of 45 minutes showed higher corrosion resistance compared to that obtained at 60 and 30 min, respectively.en
dc.formatapplication/pdfes
dc.language.isospaes
dc.publisherUniversidad Nacional de Ingenieríaes
dc.relation.ispartofseriesVolumen;22-
dc.relation.ispartofseriesNúmero;2-
dc.relation.urihttp://revistas.uni.edu.pe/index.php/tecnia/article/view/77es
dc.rightsinfo:eu-repo/semantics/openAccesses
dc.rights.urihttp://creativecommons.org/licenses/by-nc-nd/4.0/es
dc.sourceUniversidad Nacional de Ingenieríaes
dc.sourceRepositorio Institucional - UNIes
dc.subjectAluminioes
dc.subjectImpedancia electroquímicaes
dc.subjectNiebla salina ácidaes
dc.titleEstudio de la resistencia a la corrosión del Aluminio 6063 anodizadoes
dc.titleStudy of the corrosion resistance of Aluminum 6063 anodizeden
dc.typeinfo:eu-repo/semantics/articlees
dc.identifier.journalTECNIAes
dc.description.peer-reviewRevisión por pareses
dc.identifier.doihttps://doi.org/10.21754/tecnia.v22i2.77es
dc.contributor.emailpaucar@uni.edu.pees
Aparece en las colecciones: Vol. 22 Núm. 2 (2012)

Ficheros en este ítem:
Fichero Descripción Tamaño Formato  
TECNIA_Vol.22-n2-Art. 8.pdf283,78 kBAdobe PDFVisualizar/Abrir


Este ítem está sujeto a una licencia Creative Commons Licencia Creative Commons Creative Commons

Indexado por:
Indexado por Scholar Google LaReferencia Concytec BASE renati ROAR ALICIA RepoLatin UNI