Please use this identifier to cite or link to this item: http://hdl.handle.net/20.500.14076/2446
Title: Estudio metalúrgico para la separación arsenopirita-pirita en el circuito de flotación Bulk
Authors: Basurto Quinto, Andy Keith
Advisors: Suárez Sánchez, María Flor
Keywords: Recuperación de Oro;Flotación (minerales);Arsenopirita;Pirita
Issue Date: 2013
Publisher: Universidad Nacional de Ingeniería
Abstract: El relave del circuito de flotación de Zn es tratado en el circuito de flotación bulk de arsenopirita-pirita, en el cual se aplicó un método de recuperación de oro contenido mayormente en la arsenopirita. A partir del relave de zinc se realiza la flotación bulk arsenopirita-pirita, luego se realiza la flotación diferencial en caliente que consiste en flotar la arsenopirita, deprimiendo la pirita. El problema radica en la baja calidad como en la baja recuperación de oro del concentrado bulk arsenopirita-pirita que se obtenía en el circuito bulk; se diseñaron pruebas experimentales de laboratorio para llevar a cabo la separación por flotación en caliente, deprimiendo la pirita. Este resultado llevó a realizar un estudio más detallado donde se evaluaron los parámetros de trabajo más importantes que afectaban el proceso; esto se logró estableciendo el pH en un valor de 11.27 y una temperatura de 60.87 ºC en los tanques de acondicionamiento del concentrado bulk arsenopirita-pirita. De esta manera se logró incrementar la ley del oro en el concentrado de arsenopirita en un rango de 30-35 gr/Ton de Au y la recuperación del oro en el concentrado de arsenopirita se ubicó por encima del 90%.
The tailings from Zn the flotation circuit is treated in the bulk flotation circuit of arsenopyrite-pyrite, in which we applied a recovery method of gold contained mainly in arsenopyrite. Then, using zinc the tailings we performed the bulk arsenopyrite-pyrite flotation, and then we performed the differential flotation in heat consisting on floating the arsenopyrite, by depressing the pyrite. The problem is the low quality and low gold recovery, from the bulk arsenopyrite-pyrite concentrate, obtained in bulk circuit; therefore experimental tests were designed to carry out laboratory flotation separation in heat by depressing the pyrite. This result led us to perform a more detailed study which assessed the most important working parameters affecting the process; this was achieved by setting the pH to a value of 11.27 and the temperature to 60.87 ° C in the conditioning pyrite-arsenopyrite concentrate bulk tanks. Finally, we were able to increase the gold grade in the arsenopyrite concentrate in a range of 30-35 g / t Au, and gold recovery arsenopyrite concentrate was above the 90%.
URI: http://hdl.handle.net/20.500.14076/2446
Rights: info:eu-repo/semantics/restrictedAccess
Appears in Collections:Ingeniería Metalúrgica

Files in This Item:
File Description SizeFormat 
basurto_qa.pdf1,65 MBAdobe PDFView/Open


This item is licensed under a Creative Commons License Creative Commons

Indexado por:
Indexado por Scholar Google LaReferencia Concytec BASE renati ROAR ALICIA RepoLatin UNI